Civil Lab Tools / Soil Testing / CBR
California Bearing Ratio — CBR
Record the three CBR test points, soaked moisture and swell, then enter the penetration readings. CBR at 2.5 mm and 5.0 mm, the logarithmic trend and CBR at 95% MDD update as you type.
1. Test information
2. Compaction targets and equipment
The three CBR moulds normally use 2305 cm³. Use the target MDD, OMC and NMC determined from the compaction sheet for the same material.
3. CBR test points
Enter masses in grams. Pre-compaction moisture is used for the dry density; the after-soaking moisture is reported separately. Use one row per test (A, B and C).
| Parameter | Test A | Test B | Test C |
|---|
4. Penetration readings
Enter the dial gauge reading at each penetration. Force = dial reading × proving ring factor. CBR at 2.5 mm = force ÷ 13.2 × 100; CBR at 5.0 mm = force ÷ 20 × 100.
| Penetration (mm) | Test A | Test B | Test C | |||
|---|---|---|---|---|---|---|
| Dial | Force (kN) | Dial | Force (kN) | Dial | Force (kN) | |
5. CBR results
Enter the target MDD, proving ring factor and test data. Results update as you type.
| Compaction (% MDD) | Dry density (kg/m³) | CBR (%) |
|---|
The trend is CBR = a × ln(dry density) + b. It is fitted from the measured CBR points by least squares; enter a and b to use a project-specific design curve.
6. Charts
Force–penetration, CBR–density, CBR–compaction and swell–compaction charts are redrawn from the current sheet. Print in colour or save as PDF.
Force vs plunger penetration
CBR vs dry density
CBR vs compaction
Swell vs compaction
PREPARED BY
Name:
Signature: ______________________________
Date:
Assistant Materials Technician
CHECKED BY
Name:
Signature: ______________________________
Date:
Consultant's Materials Technician
VERIFIED BY
Name:
Signature: ______________________________
Date:
Consultant's Materials Engineer